Comprehensive creep compliance characterization of orthotropic materials using an automated system [0.03%] 使用自动化系统对正交各向异性和材料进行全面的蠕变性能测试
Jonas M Maas,Falk K Wittel Jonas M Maas
Determining the creep compliances of orthotropic composite materials requires experiments in at least three different uniaxial and biaxial loading directions. Up to date, data respecting multiple climates and all anatomical directions are s...
Impact of surface delignification on fire retardancy of wood treated with polyelectrolyte complexes [0.03%] 聚电解质复合物处理木材的表面脱木质素对其阻燃性的影响
Marie Soula,Fabienne Samyn,Sophie Duquesne et al. Marie Soula et al.
Wood is a natural composite widely employed as a residential building interior finishing. Although wood is readily available and offers benefits to the occupants, such as enhanced well-being, it is rarely employed in commercial construction...
Wood color modification with iron salts aqueous solutions: effect on wood grain contrast and surface roughness [0.03%] 铁盐溶液改性木色:对木材纹理对比度和表面粗糙度的影响
Roberta Dagher,Tatjana Stevanovic,Véronic Landry Roberta Dagher
Wood is a biosourced material with unique aesthetic features due to its anatomy and chemical composition. White oak wood surface color can be modified with the use of iron salts, which react with wood phenolic extractives, present as free m...
Oak wood drying: precipitation of crystalline ellagic acid leads to discoloration [0.03%] 橡木干燥:结晶丹宁酸的沉淀导致变色问题
Martin Felhofer,Peter Bock,Nannan Xiao et al. Martin Felhofer et al.
Oak heartwood usually darkens during and after drying. This darkening can be heterogeneous, leaving noncolored areas in the wood board. These light discolorations have been linked to heterogeneous distribution of tannins, but compelling evi...