Interfacial slow-release reduction modulates iron cycling on the ZVI surface: Accelerated electron transfer and generation of Fe(II)
{{output}}
Slow iron cycling is an important factor limiting the reactivity of zero-valent iron (ZVI). Developing novel strategies to facilitate iron cycling is vital for the ZVI practical application. This study reports a novel interfacial slow-release reduction strateg... ...