首页 正文

Crystal structure of (K1.5Na0.5)Ca3Si3O10

{{output}}
Single crystals of (K1.52Na0.48)Ca3Si3O10 [idealized (K1.5Na0.5)Ca3Si3O10, di(pot-assium, sodium) tricalcium tris-ilicate], were obtained from the crystallization of a glass with a molar oxide ratio of K2O:Na2O:CaO:SiO2 = 1.5:0.5:6:6 that was annealed at 1273 ... ...